Thermal treatment of a potassium-rich metamorphic rock in formation of soluble K forms
| dc.contributor.author | Santos, Wedisson Oliveira | |
| dc.contributor.author | Mattiello, Edson Marcio | |
| dc.contributor.author | Pacheco, Anderson Almeida | |
| dc.contributor.author | Vergutz, Leonardus | |
| dc.contributor.author | Souza-Filho, Luiz Francisco da Silva | |
| dc.contributor.author | Abdala, Dalton Belchior | |
| dc.date.accessioned | 2019-03-07T13:51:56Z | |
| dc.date.available | 2019-03-07T13:51:56Z | |
| dc.date.issued | 2017-02-10 | |
| dc.description.abstract | Countries like Brazil, China and India are highly dependent on external reserves of soluble potassium (K) minerals for the production of K fertilizers. On the other hand, the natural occurrence of potassium-rich silicate minerals in these countries, has seldom been commercially exploited until recently. Technological strategies that can increase the reactivity of these minerals can turn them into a resource for K fertilizer production. This work aimed to investigate the changes in solubility of Verdete rock (VR) after calcination with a melting agent (MA- CaCl2·2H2O) under varying temperatures of calcination and ratios (w w− 1) of MA/VR. Measurements of extractable K in water (Kwater), X-ray diffraction (XRD) and X-ray Absorption Near Edge Structure (XANES) were performed to identify new mineral phases. The Kwater increased up to 184-fold when the VR was calcined in the presence of MA. Optimization of calcination of VR to temperature of 850 °C and a 1.7 ratio (w w− 1) of MA/VR yielded Kwater values of up to 95% of total K. Potassium K-edge XANES analysis revealed changes in the molecular environment of K due to the calcination of VR at increasing temperatures. The K K-edge XANES fit to sylvite was supported by the detection of this mineral by XRD analysis at calcination temperatures ranging from 700 to 900 °C. In addition, K K-edge XANES analysis indicated the gradual formation of a new potassium-silicate mineral with increasing temperature, which the XANES analysis showed to be an amorphous-K2SiO3 (Amorphous-K2SiO3). The combination of Kwater and the residue of Linear Combination Fitting analysis (LCF) performed on the XANES data suggested the formation of an undefined K mineral phase additional to sylvite and Amorphous-K2SiO3. The calcination process was effective in producing highly soluble K mineral phases from a low solubility raw material. The end-products of the calcination procedure obtained in our work represent a promising alternative material for K fertilizer production, but further evaluation of the plant availability of the K in soils is needed. | en |
| dc.format | pt-BR | |
| dc.identifier.issn | 0301-7516 | |
| dc.identifier.uri | https://doi.org/10.1016/j.minpro.2016.12.004 | |
| dc.identifier.uri | http://www.locus.ufv.br/handle/123456789/23801 | |
| dc.language.iso | eng | pt-BR |
| dc.publisher | International Journal of Mineral Processing | pt-BR |
| dc.relation.ispartofseries | Volume 159, Pages 16-21, February 2017 | pt-BR |
| dc.rights | Elsevier B. V. | pt-BR |
| dc.subject | Calcination | pt-BR |
| dc.subject | Calcium chloride | pt-BR |
| dc.subject | Glauconitic rock | pt-BR |
| dc.title | Thermal treatment of a potassium-rich metamorphic rock in formation of soluble K forms | en |